Comparison of Long-Term CMAS Degradation Mechanisms of GdZrO and LaZrO Based EB-PVD Thermal Barrier Coatings
Tarih
Dergi Başlığı
Dergi ISSN
Cilt Başlığı
Yayıncı
Erişim Hakkı
Özet
Gd2Zr2O7 (GZ) and La2Zr2O7 (LZ) thermal barrier coatings were deposited by electron beam physical vapor deposition (EB-PVD) on cold gas dynamic sprayed CoNiCrAlY bond coats over Inconel 718 substrates. The systems were exposed to a vermiculite-derived silicate deposit at 1250 degrees C for nominal holding times of 4-32 h and examined by SEM, EDS, and XRD. Both systems exhibited intercolumnar infiltration, reduced measured porosity, increasing local hardness, oxide growth, and eventual loss of the continuous ceramic layer. Pronounced fragmentation was observed in the 16 h GZ specimen, and no continuous GZ topcoat was observed at the 20 h condition. A continuous LZ layer remained identifiable at 20 h, whereas the continuous layer was absent at 24 h. These are post-test observations from different specimens, not exact failure times. Diffraction features assigned to silicate phases and residual zirconates were interpreted together with the microstructural observations; residual zirconate peaks do not demonstrate preservation of a continuous coating. The examined LZ specimens retained a continuous ceramic layer to a later sampled exposure condition than the GZ specimens. This qualitative comparison is limited by one specimen per coating-time condition, discrete 4 h sampling and the absence of deposit-free controls, which prevents separation of thermal aging from deposit-assisted degradation.