Dunite powder as a green precursor in one-part alkali-activated composites: Effects on mechanical and durability properties

dc.contributor.authorBenli, Ahmet
dc.contributor.authorBayraktar, Oguzhan Yavuz
dc.contributor.authorKaratas, Mehmet
dc.contributor.authorBodur, Burak
dc.contributor.authorYilmazoglu, Mehmet Ugur
dc.contributor.authorKaplan, Gokhan
dc.contributor.authorBodur, Burak
dc.date.accessioned2025-10-18T10:00:02Z
dc.date.created2025
dc.date.issued2025
dc.departmentBartın Üniversitesi
dc.description.abstractNatural pozzolans are a sustainable alternative to Portland cement, offering abundant alumina and reactive silica for geopolymer production. Due to their simple extraction methods, they are cost-effective and environmentally friendly. This study explores the utilization of dunite powder (DP) as a sustainable precursor in one-part alkali-activated slag-based composites (AAC), aiming to evaluate its potential to partially replace granulated blast furnace slag (GBFS). The mechanical, fresh, and durability properties of the composites were investigated by varying DP replacement levels (0%, 15%, 30%, and 60%) under an activator dosage of sodium metasilicate, with the mixtures cured at 80 degrees C for 24 h and subsequently exposed to ambient conditions. The compressive and flexural strengths were evaluated at 7, 28, and 91 days, while the fresh properties (flowability and setting time), durability under sulfate attack, high-temperature resistance, freeze-thaw resistance, dry shrinkage, sorptivity and microstructural characteristics (SEM, XRD, and FT-IR) were also examined. The compressive strength decreased with higher DP content, with the 60% DP mixture showing a 43% strength reduction at 28 days compared to the reference mixture. However, the 30% DP mixture achieved a favorable balance between strength and sustainability, demonstrating a compressive strength decrease of only 11% at 91 days. The mixture containing 15% DP demonstrated the best performance under high-temperature conditions and freeze-thaw cycles. The 60% DP mixture exhibited the highest mass and strength loss when exposed to temperatures above 400 degrees C and a 15% compressive strength reduction after 120 days of immersion in a 10% MgSO4 solution.
dc.identifier.doi10.1016/j.scp.2025.101964
dc.identifier.issn2352-5541
dc.identifier.orcidKaplan, Gokhan/0000-0001-6067-7337;
dc.identifier.scopus2-s2.0-85218117438
dc.identifier.scopusqualityQ1
dc.identifier.urihttps://doi.org/10.1016/j.scp.2025.101964
dc.identifier.urihttps://hdl.handle.net/11772/20044
dc.identifier.volume44
dc.identifier.wosWOS:001430980400001
dc.identifier.wosqualityN/A
dc.indekslendigikaynakWeb of Science
dc.indekslendigikaynakScopus
dc.language.isoen
dc.publisherElsevier
dc.relation.ispartofSustainable Chemistry and Pharmacy
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanı
dc.relation.sdgGoal-12: Responsible Consumption and Production
dc.rightsinfo:eu-repo/semantics/closedAccess
dc.snmzWoS_20251016
dc.subjectDunite Powder
dc.subjectAlkali-Activated Composites
dc.subjectGranulated Blast Furnace Slag
dc.subjectSustainable Construction
dc.subjectMechanical And Durability Properties
dc.titleDunite powder as a green precursor in one-part alkali-activated composites: Effects on mechanical and durability properties
dc.typeArticle
dspace.entity.typePublication
relation.isAuthorOfPublicationf382b3b5-179f-4199-b4bc-7f296011bd1e
relation.isAuthorOfPublication.latestForDiscoveryf382b3b5-179f-4199-b4bc-7f296011bd1e

Dosyalar