In this study, Trapa natans nut collected from the costs of Inkumu-Bartin was analyzed according to its lignin content.Acid-insoluble lignin content was determined according to TAPPI T222om-02 as 28.31%. TGA and FTIR analyses were performed.FTIR analysis indicated that Trapa natans contained cellulose, hemicelluloses and lignin. The peaks at 1506-1510 cm-1in bothsamples are characteristic peaks for the lignin components due to C = O and COO-non-symmetric stretching vibrations in the aromatic rings ofthe lignin structure. 1510 cm-s peak is found in the literature as lignin’s fingerprint peak. The peaks at 1230-1270 cm-1 band show the vibrationsof guayasil ring with CO tension in lignin and hemicelluloses. Around the peaks of 900, 1025, 1030 and 1050 cm-1 bands cellulose’s O-H, C-Hand C-O-C type bonds are seen. When TGA analyzes are examined, approximately 4.5% of the sample is lost from 30 °C to 200 °C. At theseintervals, samples generally lose volatile constituents and moisture. From 200 to 271 °C 4.6% of the weight is lost. The decrease in this rangemay be due to the decomposition of cellulose and hemicelluloses. The DTG curve shows maxima weight-loss occurring at 349 °C. The weightloss in the range from 271-352 °C is about 50%. Pure lignin sample’s TGA and DTG curve results show 10%, 50%, and 70% weight-losses at233 °C, 489 °C, and 1167 °C respectively. According to these results, dominantly lignin and small quantities of cellulose and hemicelluloses arepresent in trapa samples.

Açıklama

Anahtar Kelimeler

Kimya, Uygulamalı, Kimya, Organik

Kaynak

JOURNAL OF ANATOLIAN ENVIRONMENTAL AND ANIMAL SCIENCES

WoS Q Değeri

Scopus Q Değeri

SDG

Cilt

4

Sayı

4

Künye

Onay

İnceleme

Ekleyen

Referans Veren