Recovery of precious metals from spent Mo-Co-Ni/Al2O3 catalyst in organic acid medium: Process optimization and kinetic studies

dc.contributor.authorArslanoglu, Hasan
dc.contributor.authorYaraş, Ali
dc.contributor.authorYaraş, Ali
dc.date.accessioned2025-10-18T10:07:25Z
dc.date.created2019
dc.date.issued2019
dc.departmentFakülteler, Mühendislik Mimarlık ve Tasarım Fakültesi, Metalurji ve Malzemem Mühendisliği Bölümü
dc.description.abstractIn present study, the leaching kinetics of the spent Mo-Co-Ni/Al2O3 catalyst was investigated in the presence of formic acid as an organic leaching agent. Firstly, the spent catalyst was roasted in different roasting temperature (200-700 degrees C) and time (15-240 min), the maximum metal extraction was achieved that at 500 degrees C with 90 min. Then, the leaching experiments were carried out to determine the influences of process parameters following; particle size, liquid/solid ratio, formic acid concentration, leaching temperature, leaching time and stirring speed. According to the experimental results, the highest dissolution rates of molybdenum (Mo, 75.82%), cobalt (Co, 96.81%), nickel (Ni, 93.44%) and aluminum (Al, 19.46%) were reached under optimum experimental conditions; particle size thorn75 degrees 30 mm; liquid/ solid ratio 10 ml/g; formic acid concentration 0.6M; leaching temperature 80 degrees C; leaching time 90 min and stirring speed 300 r/min. Moreover, the leaching kinetics clearly reveal that the leaching reaction is controlled by liquid film diffusion and that the activation energy values (Ea) of Co, Ni, Mo and Al were to be 24.49, 25.98, 32.36 and 33.47 kJ/mol, respectively. In conclusion, the leaching process can be conducted in the presence of formic acid for the various industrial wastes in similar structure and composition to Mo-Co-Ni/Al2O3 spent catalyst.
dc.identifier.doi10.1080/10916466.2019.1618867
dc.identifier.endpage2093
dc.identifier.issn1091-6466
dc.identifier.issn1532-2459
dc.identifier.issue19
dc.identifier.orcidArslanoglu, Hasan/0000-0002-3132-4468
dc.identifier.orcidYaras, Ali/0000-0003-1725-7788;
dc.identifier.scopus2-s2.0-85066068953
dc.identifier.scopusqualityQ2
dc.identifier.startpage2081
dc.identifier.urihttps://doi.org/10.1080/10916466.2019.1618867
dc.identifier.urihttps://hdl.handle.net/11772/21556
dc.identifier.volume37
dc.identifier.wosWOS:000469044700001
dc.identifier.wosqualityQ3
dc.indekslendigikaynakWeb of Science
dc.indekslendigikaynakScopus
dc.language.isoen
dc.publisherTaylor & Francis Inc
dc.relation.ispartofPetroleum Science and Technology
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanı
dc.rightsinfo:eu-repo/semantics/closedAccess
dc.snmzWoS_20251016
dc.subjectSpent Catalyst
dc.subjectMolybdenum
dc.subjectCobalt
dc.subjectNickel
dc.subjectLeaching
dc.subjectKinetic
dc.titleRecovery of precious metals from spent Mo-Co-Ni/Al2O3 catalyst in organic acid medium: Process optimization and kinetic studies
dc.typeArticle
dspace.entity.typePublication
relation.isAuthorOfPublication58d7c06e-c79d-4315-b765-30c20697856b
relation.isAuthorOfPublication.latestForDiscovery58d7c06e-c79d-4315-b765-30c20697856b

Dosyalar