Pack-Boriding of Monel 400: Microstructural Characterization and Boriding Kinetics

Yükleniyor...
Küçük Resim

Tarih

Dergi Başlığı

Dergi ISSN

Cilt Başlığı

Yayıncı

Korean Inst Metals Materials

Erişim Hakkı

info:eu-repo/semantics/closedAccess

Araştırma projeleri

Organizasyon Birimleri

Dergi sayısı

Özet

Monel 400 was pack-borided in the temperature range of 1173-1273 K for exposure times of 2-6 h. The boride layers produced on the surface of the alloy were examined by scanning electron microscopy and phase identification was carried out by X-ray diffraction. The topmost layer on the borided Monel 400 was compact and contained the Ni2B phase while the diffusion zone contained grain boundary precipitates of borides. Boride layers of 35-290 mu m thickness and 1002-1476 HV0.025 hardness were obtained. SEM observations revealed a smooth interface between the boride layer and the diffusion zone. A kinetic model based on the integral method was applied to investigate the kinetics of Ni2B layer. The boron activation energy in the Ni2B layer was estimated as equal to 300.7 kJ mol(-1). An experimental validation of the model was made by comparing the experimental layer thicknesses obtained, after boriding at 1198 K for 1 and 3 h, with predicted values. [GRAPHICS] .

Açıklama

Anahtar Kelimeler

Superalloy, Monel 400, Boriding, Integral Diffusion Model

Kaynak

Metals and Materials International

WoS Q Değeri

Scopus Q Değeri

SDG

Cilt

28

Sayı

8

Künye

Onay

İnceleme

Ekleyen

Referans Veren