dc.contributor.author | Uzun, Orhan | |
dc.contributor.author | Yılmaz, Fikret | |
dc.contributor.author | Emeksiz, Cem | |
dc.contributor.author | Ergen, Semra | |
dc.contributor.author | Köleman, Uğur | |
dc.date.accessioned | 2019-03-01T08:36:56Z | |
dc.date.available | 2019-03-01T08:36:56Z | |
dc.date.issued | 2018 | |
dc.identifier.citation | Uzun, O., Yılmaz, F., Ergen, S., Emeksiz, C., Kolemen, U. (2018) Correlation of Hardness and Silicon Morphology For Al-Si-Sb Alloy”Archives Of Metallurgy and Materials, 63 (1), 467-472 | en_US |
dc.identifier.issn | 1733-3490 | |
dc.identifier.uri | http://journals.pan.pl/dlibra/publication/118963/edition/103513/content | |
dc.identifier.uri | http://hdl.handle.net/11772/520 | |
dc.description.abstract | In this study, we have focused on the role of silicon morphology on the hardness of eutectic Al – 12 wt.% Si – 0.5 wt.% Sb alloy solidified at different cooling rates. The alloys were produced by using induction melting, arc-remelting and melt-spinning techniques. The cooling rates of the alloys were determined as 0.5, 60 and ~105°C.s–1 for induction-melted, arc-remelted and meltspun alloy. The experimental results show that as the cooling rate increased the coarse silicon phase was substantially refined and its morphology altered from sharp need-like to round shape. Two exothermic peaks, attributed to precipitation and coarsening of silicon from supersaturated α-Al, were observed in the DSC curve of MS alloy. Vicker’s hardness of melt-spun alloy was found two times higher than those of IMed and ARed alloys. The lowest hardness of induction-melted alloy was ascribed to the lamellar morphology of silicon, yielding decohesive rupture. This result was confirmed by finite element analyzing. Keywords: Al-Si alloy; casting; Vickers; finite element analysis | en_US |
dc.language.iso | eng | en_US |
dc.publisher | Archives of Metallurgy and Materials | en_US |
dc.relation.isversionof | 10.24425/118963 | en_US |
dc.rights | info:eu-repo/semantics/openAccess | en_US |
dc.subject | Al-Si alloy | en_US |
dc.subject | Casting | en_US |
dc.subject | Vickers | en_US |
dc.subject | Finite element analysis | en_US |
dc.subject | Al-Si alaşımı | en_US |
dc.subject | Döküm | en_US |
dc.subject | Sonlu elemanlar analizi | en_US |
dc.title | Correlation of hardness and silicon morphology for al-si-sb alloy | en_US |
dc.type | article | en_US |
dc.relation.journal | Archives of Metallurgy and Materials | en_US |
dc.contributor.department | Bartın Üniversitesi, Rektörlük | en_US |
dc.contributor.authorID | https://orcid.org/0000-0001-7586-9075 | en_US |
dc.contributor.authorID | Scopus ID: 7007089321 | en_US |
dc.identifier.volume | 63 | en_US |
dc.identifier.issue | 1 | en_US |
dc.identifier.startpage | 467 | en_US |
dc.identifier.endpage | 472 | en_US |